石化工业炉通用不定形耐火材料指标 | ||||||
材料名称 | 体积密度 (g/cm3) | 冷态耐压强度(MPa) | 冷态抗折强度(MPa) | 815℃烧后线变化率(%) | 350℃导热系数(W/m.k) | |
110℃ | 110℃ | 815℃ | 110℃ | |||
WHL-Q0.5 | ≤0.50 | ≥1.5 | ≥1.2 | ≥0.6 | 0~-0.6 | ≤0.15 |
WHL-Q0.7 | ≤0.70 | ≥2.2 | ≥1.8 | ≥0.7 | 0~-0.55 | ≤0.17 |
WHL-Q0.8 | ≤0.80 | ≥2.6 | ≥2.1 | ≥0.8 | 0~-0.50 | ≤0.21 |
WHL-Q0.9 | ≤0.90 | ≥3.0 | ≥2.5 | ≥1.0 | 0~-0.50 | ≤0.23 |
WHL-Q1.0 | ≤1.00 | ≥4.0 | ≥3.5 | ≥1.3 | 0~-0.45 | ≤0.25 |
WHL-Q1.2 | ≤1.20 | ≥5.0 | ≥4.5 | ≥1.5 | 0~-0.40 | ≤0.30 |
WHL-Q1.3 | ≤1.30 | ≥6.0 | ≥5.0 | ≥2.0 | 0~-0.30 | ≤0.35 |